A conformal coating is a thin, protective polymer film applied over electronic assemblies to defend against moisture, chemicals, dust, and other environmental hazards. What makes it “conformal” is its unique ability to follow the exact contours and geometries of complex PCBs and components, forming a seamless, invisible barrier without altering the design or function of the assembly.

Conformal coatings extend the functional life of electronics by preventing corrosion, contamination, and short circuits. They also contribute to product ruggedness, reduce field failure rates, and help manufacturers meet extended warranty commitments and regulatory reliability standards.

Conformal Coatings Available at KRAYDEN

KRAYDEN offers a wide range of conformal coatings based on different chemistries, including acrylics, silicones, synthetic rubbers, and UV-curable acrylates. Each chemistry offers distinct properties suited for specific application requirements, such as electrical insulation, moisture resistance, chemical protection, or mechanical flexibility.

These coatings are also available with varied curing mechanisms (e.g. moisture, heat, UV), allowing compatibility with different production speeds and process constraints.

For application-specific recommendations or technical support, feel free to get in touch. Contact us →

138 products

Product selector guide

Polyurethane Conformal Coatings

Product Film Thickness (μm) Cure Type Glass Transition Temperature Tg (℃) Viscosity (mPa·s) Dielectric Strength (kV/mm) Dielectric Constant / Dissipation Factor
Humiseal 1A20R 25-75 24 hrs @ RT or 3 hrs @76°C 71 100 - 3.5/0.028 at 1 MHz
Humiseal 1A27 25-75 30 days at RT or 30 hours @ 76°C or 20 hours @88°C  28 3,000 - 3.6/0.02  at 1 MHz
Humiseal 1A27LU 25-75 30 days at RT or 30 hours @ 76°C or 20 hours @88°C  28 1700 - 3.6/0.02  at 1 MHz
Humiseal 1A33 Varies RT (30 days) or 88℃ (20h) 54 180 - 3.6/0.03  at 1 MHz
Humiseal 1A33 GEL Varies 30 days at RT 30 hours @76°C 20 hours @87°C - - 42 -
Humiseal 1A68 25-75 30 days at RT or 30 hours @ 76°C or 20 hours @88°C 26 180 - 3.6/0.03  at 1 MHz
Humiseal 2A64 25-75 3 hrs @76°C 12 130 - 3.5/0.024  at 1 MHz
Loctite Stycast PC18M Varies Air-dried 30 to 45 minutes prior to curing 2 hours @60°C - - - 4.2/0.01  at 100 kHz

 

Acrylic Conformal Coatings

Product Film Thickness (μm) Cure Type Glass Transition Temperature Tg (℃) Viscosity (mPa·s) Dielectric Constant / Dissipation Factor
Humiseal 1B12 25-75 24 hrs @ RT or 30 min @76°C 32 30 2.8/0.01 at 1 MHz
Humiseal 1B15 25-75 24 hrs @ RT or 30 min @76°C 15 470 2.03/0.01 at 1 MHz
Humiseal 1B31 25-75 24 hrs @ RT or 30 min @76°C 14 200 2.5/0.01 at 1 MHz
Humiseal 1B66 25 - 75 24 hrs @ RT or 30 min @76°C  14 200 2.5/0.01 at 1 MHz
Humiseal 1B73 Varies RT (24h) or 76℃ (2h) 42 250 2.6/0.01 at 1 MHz
Humiseal 1R32 25 - 75 24 hrs @ RT or 30 min @76°C -65 220 2.5/0.01 at 1 MHz
Humiseal 1R32A-2 25-75 24 hrs @ RT or 2 hrs @76°C  14 Varies 2.5/0.01 at 1 MHz
Loctite Stycast PC 62 25 - 100  24 hours@25°C or 45 minutes @75°C - 52 -

 

Silicone Conformal Coatings

Product Film Thickness (μm) Cure Type Glass Transition Temperature Tg (℃) Viscosity (mPa·s) Dielectric Constant / Dissipation Factor
Humiseal 1C49 50 - 200 24 hrs @ RT or 20 min @76°C -65 9000 2.5/0.01 at 1 MHz
Humiseal 1C49LV 50 - 200 24 hrs @ RT or 20 min @76°C -65 550 2.5/0.01 at 1 MHz
Humiseal 1C51 50 - 200 10 - 15 minutes @105 - 130ºC  -65 630 2.4/0.01 at 1 MHz
Humiseal 1C53 50 - 200 10 - 15 min @105 - 130ºC -65 590 2.4/0.01 at 1 MHz
Humiseal 1C55 50 - 200 10 - 15 minutes @ 105 - 130ºC -65 195 - 400 2.4/0.01 at 1 MHz
Humiseal 1C63 Varies 24 hrs @ RT or 20 min @ 76°C -90 3500 -
Humiseal 2C51 Varies 30 minutes @70°C or 60 min RT  - 275/550 -
Loctite SI 5293 Varies Minimum irradiance of 70 mW/cm2 for approximately 20 to 40 seconds - 400 - 800 4.5 / 0.014 at 1 MHz

 

Synthetic Rubber Conformal Coatings

Product Film Thickness (μm) Cure Type Glass Transition Temperature Tg (℃) Viscosity (mPa·s) Dielectric Strength (kV/mm) Dielectric Constant / Dissipation Factor
Humiseal 1B51 25-75 24 hrs @ RT or 30 min @76°C 14 185 - 2.5/0.07 at 1 MHz
Humiseal 1B51LU 25-75 24 hrs @ RT or 30 min @76°C 14 185 - 2.5/0.07 at 1 MHz
Humiseal 1B51NS 25-75 24 hrs @ RT or 30 min @76°C 14 185 - 2.5/0.07 at 1 MHz
Humiseal 1B51NSLU 25-75 RT (24h) or 76℃ (2h) 14 60 - 2.5/0.07 at 1 MHz
Humiseal 1B58LU-60 25-75 24 hrs @ RT or 30 min @76°C -49.6 60 138 1.9/0.0068 at 1 MHz

 

Acrylate Conformal Coatings

Product Film Thickness (μm) Cure Type Glass Transition Temperature Tg (℃) Viscosity (mPa·s) Dielectric Constant / Dissipation Factor
Humiseal UV20 GEL -  LED system with wavelength of 395nm and power >12W 31 Highly thixotropic material -
Humiseal UV40 25-125 Arc and Microwave-based UV curing 45 650 2.5/0.01 at 1 MHz
Humiseal UV40HV - Arc and Microwave-based UV curing 45 3700 2.5/0.01 at 1 MHz
Humiseal UV40 LED 25-125  Lamp units >8w/cm2 at 385nm (14 W) or 395nm (12W) -2.4 650 -
Humiseal UV40 SOLAR 25-125 Arc and Microwave-based UV curing 45 650 2.5/0.01 at 1 MHz
Humiseal UV50LV 25-125 Arc and Microwave-based UV curing -1 80 -
Humiseal UV92 - UV-LED at 365nm or 405nm  - Thixotropic paste -
Loctite Stycast PC 40-UMF -  10 seconds @ 300 to 600 mW/cm² at 365nm - 250 2.75/0.12 at 1 MHz

 

Epoxy Conformal Coatings

Product Film Thickness (μm) Cure Type Glass Transition Temperature Tg (℃) Viscosity (mPa·s) Dielectric Strength (kV/mm) Dielectric Constant / Dissipation Factor
Humiseal 2A53 25-75  2 hrs @ 93°C 19 350 - 3.0/0.03 at 1 MHz

 

Frequently asked questions

Frequently Asked Questions about Conformal Coatings

How is a conformal coating applied?

There are multiple ways to apply a conformal coating, all based on the specifics of the application. Some common methods include:

  • Hand Brushing
  • Hand Dispensing
  • Spray Coating (Aerosol or Handspray)
  • Dip Coating
  • Selective Coating

How does conformal coating work?

The liquid coating “conforms” to every contour of the assembly, creating a continuous protective film that shields components from moisture, dust, chemicals, and electrical leakage.

How do I choose the right conformal coating chemistry?

Selection depends on environmental stresses, thermal range, humidity, mechanical stress, chemical exposure, and reworkability needs. For example:

  • Acrylics – easy to apply and rework, limited high-temp resistance
  • Silicones – excel in high-humidity, high-temp, vibration-heavy environments
  • Polyurethanes – resist solvents and abrasion
  • UV-curable – ideal for high-speed, inline production

Can conformal coatings be applied selectively?

Yes. Automated selective coating equipment can precisely deposit coating only on critical areas—leaving connectors, test points, or sockets exposed—reducing masking and cleanup.

What surface preparation is required?

Cleanliness is critical. Assemblies must be free of flux residues, oils, and particulates—often requiring plasma cleaning, ionized air, or aqueous washing. IPC-CC-830 recommends ionic contamination <1.56 µg/cm² NaCl equivalent.

How do coatings perform under thermal cycling and stress?

Performance varies by chemistry:

  • Silicones – best for –55 °C to +200 °C cycles, handle vibration without cracking
  • Acrylics/Epoxies – may crack or delaminate under extreme flex or rapid thermal change

Learn more

Conformal Coatings

Thin polymeric films applied to electronic circuits and components to protect them from environmental conditions, such as:

  • Moisture and humidity
  • Dust and chemicals
  • Corrosive atmospheres (e.g., salt spray)
  • Temperature extremes

They “conform” to the shape of the board and its components — hence the name — forming a protective barrier without affecting the function of the electronics.

Conformal coating
Moisture barrier for corrosion and short-circuit prevention
Electrical insulation and chemical shielding
Full coverage across complex and irregular geometries
UV-traceable for easy inspection and defect detection
Why use conformal coating

Why is conformal coating used?

Conformal coatings are highly recommended to use in PCBs for a multitude of reasons, including the following:

  • Circuit size reduction & high component densities
  • Keeps debris away from sensitive components
  • Extended warranties
  • Improvement in reliability
  • Increased customer satisfaction
  • Protection from harsh environements
  • Protection against electrochemical migration (i.e., formation of dendrites between 2 components tracks as a result of resence of an electrolyte such as water)

Protecting Electronics Across Industries

Conformal coatings are essential in industries where electronic reliability is critical under environmental stress. From automotive to aerospace, consumer tech to medical equipment, these coatings form a thin, invisible shield that protects sensitive circuitry from moisture, dust, chemicals, and thermal extremes, enhancing performance, safety, and service life.

 

 

Consumer Electronics

Smartphones, wearables, home devices

Automotive

ECUs, sensors, lighting modules

Industrial

Control systems, IoT nodes

Aerospace & Defense

Avionics, guidance systems

 

Conformal Coating Product Ecosystem

The effectiveness of a conformal coating system relies not only on the coating itself but also on the complementary products that ensure precise application, consistent performance, and easy rework. A typical ecosystem includes:

 

Conformal Coating

  • Uniform, thin protective barrier
  • Prevents moisture, dust, corrosion

Chemistries:

  • Acrylics
  • Silicones
  • Urethanes
  • UV-curable
Conformal Coating
Thinner

Thinner

  • Adjusts spray, dip or brush viscosity
  • Ensures uniform film thickness

Selection:

  • Match solvent blends to each chemistry
  • Balance thinning vs. adhesion

Stripper

  • Removes cured coatings safely
  • No damage to sensitive components

Types:

  • Fast-acting solvents for bulk
  • Gentle spot-stripping formulas
Stripper
Masking Materials

Masking Materials

  • Protects connectors & test points
  • Leaves critical areas coating-free

Options:

  • Liquid masks
  • Peelable tapes
  • Silicone plugs

 


 Types of Conformal Coatings According to Chemistry of Base Resin

Conformal coatings come in several chemistries, each offering unique protective properties and application characteristics suited for different environments and industry needs. The most common types include acrylic, silicone, polyurethane, epoxy, and parylene coatings. These materials vary in terms of moisture resistance, chemical durability, flexibility, ease of application, and reworkability, making the selection dependent on the specific performance demands of the application.

 

Acrylic

Pros: Easy to apply and remove; dries quickly and is cost-effective for general use.

Cons: Limited chemical and temperature resistance; not ideal for harsh or high-performance environments.

Urethane

Pros: Strong resistance to moisture, chemicals, and abrasion; good for automotive or industrial use.

Cons: Rigid and harder to rework; long curing times and possible outgassing issues.

Silicone

Pros: Excellent flexibility and thermal stability; ideal for high-temperature or outdoor use.

Cons: Difficult to remove or rework; may have limited chemical resistance depending on formulation.

Rubber

Pros: Cost-effective coating with balanced performance for less demanding environments.

Cons: Limited high-temperature resistance; moderate chemical resistance.

 

Conformal Coating Selector Guide based on Resin Chemistry

Acrylic conformal coatings are typically based on polymers derived from acrylic acid or methacrylic acid esters. These resins are linear and thermoplastic, which means they do not crosslink during curing. This gives them high reworkability and allows for fast curing.

Acrylic-based coatings represent the largest market share of conformal coatings. The widespread choice of acrylics can be attributed to their ease of use, short cure time, and reworkability/repairability.

Polyurethane coatings are formed by crosslinking polyols with isocyanates, resulting in a flexible, tough layer with excellent abrasion and chemical resistance. Compared to acrylics, polyurethanes offer higher chemical resistance and mechanical strength, second only to epoxies. However, they remain easier to rework than epoxies and stand up well to salt spray and industrial gases. Note that polyurethane coatings typically require longer curing times.

Silicone-based conformal coatings are uniquely characterized by their exceptional high-temperature performance. The strong, thermally stable Si–O bonds in silicones outperform the carbon–carbon bonds found in acrylics, enabling these coatings to withstand temperatures above 150 °C. They excel in applications like industrial mining equipment, high-temperature electronics, and underhood automotive components.

While silicones are not as abrasion-resistant due to their rubbery flexibility, this same property allows them to absorb vibration. Removal typically requires specialized solvents, prolonged soak times, and mechanical agitation.

Synthetic rubber conformal coatings are elastomer-based films, often made from butyl rubber or styrene block copolymers. They offer moderate reworkability and good moisture resistance. Though not as chemically or thermally robust as polyurethanes or silicones, they deliver balanced performance for less demanding environments and withstand vibration and damping stresses well.

selection network

Acrylic
Reworkability
★★★★☆
Moisture Resistance
★★☆☆☆
Chemical Resistance
★★☆☆☆
Thermal Resistance
★★☆☆☆
Dielectric Strength
★★★★☆
Cost
$
Best for automotive, avionics, communications, fast repair, reworkable systems
Polyurethane
Reworkability
★★☆☆☆
Moisture Resistance
★★★★☆
Chemical Resistance
★★★★★
Thermal Resistance
★★★☆☆
Dielectric Strength
★★★★☆
Cost
$$
Best for shipping, avionics, chemical process, industrial harsh zones
Silicone
Reworkability
★★☆☆☆
Moisture Resistance
★★★★★
Chemical Resistance
★★★☆☆
Thermal Resistance
★★★★★
Dielectric Strength
★★★★★
Cost
$$$
Best for high-temp circuits, LED lighting, solar inverters
Rubber
Reworkability
★★☆☆☆
Moisture Resistance
★★★★☆
Chemical Resistance
★★★☆☆
Thermal Resistance
★★★☆☆
Dielectric Strength
★★★☆☆
Cost
$
Best for automotive, transportation, rail, high temp, vibration-prone, low-cost devices, LED drivers
UV-curable (Acrylates)
Reworkability
★★☆☆☆
Moisture Resistance
★★☆☆☆
Chemical Resistance
★★★★☆
Thermal Resistance
★★★☆☆
Dielectric Strength
★★★★☆
Cost
$$
Best for high-volume, inline production, VOC-sensitive processes

 Types of Conformal Coatings According to Curing Mechanisms

Solvent Evaporation

Solvent Evaporation

Film cures as dissolved resin solids deposit when the solvent (or water) flashes off at room temperature or with mild heat.

Acrylics
Synthetic Rubbers

Moisture Cure

Moisture Cure

One-part formulations that crosslink when ambient moisture diffuses into the film and triggers polycondensation or addition.

Silicones
Polyurethanes

Heat Cure

Heat Cure

Requires elevated temperature (often 80–150 °C) to drive crosslinking reactions in the absence of UV or moisture.

Two-part Epoxies
2K Polyurethanes

UV Cure

UV Cure

Uses photoinitiators that, upon UV absorption, generate radicals or cations to rapidly polymerize acrylate-based resins.

Multifunctional Acrylates
Epoxy-modified Acrylates

Dual Cure

Dual Cure

Combines two mechanisms (e.g., UV + moisture, UV + thermal) to ensure cure in shaded areas or to boost final properties.

Hybrid Chemistries
(e.g., Acrylate + Silicone)

 


UV-curable Conformal Coatings

UV-curable conformal coatings are thin polymeric films applied to electronic assemblies that rapidly crosslinks and solidifies when exposed to ultraviolet (UV) light. This technology addresses the length cure cycles and complications on solvent handling required in early conformal coatings. UV-curable coatings are typically multifunctional acrylates or epoxy-modified acrylates that provide hardness and chemical resistance.

Another processing advantage is that this technology is environmentally friendly, as it contains no volatile organic compounds (VOCs) or solvents. Like silicone coatings, it is 100% solid. Due to the short cure time, UV-curable conformal coatings are suitable for high-volume applications.

Key Features

  • UV cure in seconds
  • Eliminates bake/flash steps
  • High chemical resistance; moderate moisture barrier
  • Tough yet flexible; abrasion-resistant
  • 100 % solids; zero VOC/solvent
  • Compact UV stations (no ovens)
  • Optimized for high-volume inline lines
  • Hybrid chemistries (acrylate, PU, epoxy blends)
 

Best Use Cases

  • High-volume, fast-turnaround production
  • Temperature-sensitive components
  • Selective / mask-free coating
  • Complex geometries and fine-pitch boards
  • Flexible and wearable electronics
  • Optoelectronic and sensor modules
  • Field service and touch-up
  • Automotive electronics (under-hood / high-vibe)
  • Miniaturized and micro-assembly
  • Hybrid cure strategies

UV-curable Conformal Coatings Cure Mechanism

 

Pre-cure
Before any UV exposure, the coating exists as a uniform, liquid film composed of linear oligomer and monomer chains, photoinitiator molecules, and some additives.

→

 

UV Light Exposure and Absorption

Photoinitiator molecules absorb UV photons and cleave (radical cure) or generate cations (cationic cure). These reactive species are the “spark” that starts chain-growth polymerization of the acrylate/epoxy groups.

→

 

Crosslinking

Multifunctional acrylates link together, forming a three-dimensional network. Within seconds, viscosity spikes as the network percolates, and the film becomes tack-free.

 

 


Dual-cure Conformal Coatings

Dual-cure conformal coatings are hybrid systems engineered to combine two distinct curing mechanisms, typically a rapid primary cure (such as UV-initiated polymerization) and a secondary cure (moisture- or heat-driven crosslinking), to deliver both instant handling strength and complete, through-film cure even in shadowed or occluded regions.

Best Use Cases

  • Complex Assemblies: High-pin-count PCBs, connectors, and sensors where full 3D coverage is critical.
  • High-Reliability Electronics: Automotive ECUs, medical instruments, and aerospace modules needing both instant cure and long-term durability.
  • Inline Production Lines: Facilities seeking to maximize throughput without sacrificing cure completeness or film integrity.
Dual-cure coatings illustration

Conformal Coatings Cheat Sheet,
Classification by Cure Mechanism, Typical Chemistries, and Solvent Content

Cure Mechanism Typical Chemistries Contains Solvent?
Solvent Evaporation Organic-solvent acrylics Yes
Waterborne acrylics Yes
Synthetic rubbers Yes
Solvent-based polyurethanes Yes
Solvent-borne hybrids Yes
Moisture Cure 1-part RTV silicones No
1-part moisture-cure polyurethanes No
Heat Cure 2-part epoxies No
2-part polyurethanes Varies
Cationic epoxies (thermal post-cure) No
Photo-Initiated (UV-Cure) Multifunctional acrylates No
UV-curable epoxy-acrylates No
Dual-Cure / Hybrid UV-acrylate + moisture-cure silicones No
UV-acrylate + thermal-cure epoxies No

Conformal Coating Application Methods

Applying a conformal coating isn’t a one-size-fits-all decision. If you’re running dozens or thousands of boards, a high-speed spray booth can blanket them in seconds. Need pinpoint accuracy? Robotic dispensers or stencil masks let you coat just the connectors and test points. Dip coating delivers an even film over every surface, while a simple brush or stencil approach is ideal for prototypes and spot repairs. And when only certain areas require protection, selective coating cuts down on waste and cleanup. Ultimately, the best choice comes down to your board’s shape, how tightly you’ve packed components, your production volumes, and how consistent that coating needs to be, so you protect your electronics without slowing down your workflow.

 

Hand Brush
Uniformity
★☆☆☆☆
Throughput
★☆☆☆☆
Wastage
★★★★★
Masking Req.
★★★★☆
Ideal Batch Size
1–10 pcs
Cost
$
Best for prototypes, rework/repair, small batches
Hand Dispensing
Uniformity
★★☆☆☆
Throughput
★★☆☆☆
Wastage
★★★★★
Masking Req.
★★★★☆
Ideal Batch Size
1–20 pcs
Cost
$
Best for selective spot coating, rework/touch up
Hand-held Spray
Uniformity
★★☆☆☆
Throughput
★★☆☆☆
Wastage
★☆☆☆☆
Masking Req.
★★★☆☆
Ideal Batch Size
10–100 pcs
Cost
$$
Best for small to medium batches, field servicing, maintenance
Selective Coating
Uniformity
★★★★★
Throughput
★★★★☆
Wastage
★★★★★
Masking Req.
★★★★★
Ideal Batch Size
up to 100 pcs
Cost
$$$$$
Best for coating only critical “hot spots,” stencil-style patterns
Automated Dip
Uniformity
★★★★★
Throughput
★★★☆☆
Wastage
★★★★★
Masking Req.
★★☆☆☆
Ideal Batch Size
50–500 pcs
Cost
$$$
Best for high-volume yields where overspray must be avoided
Automated Spray
Uniformity
★★★★☆
Throughput
★★★★★
Wastage
★☆☆☆☆
Masking Req.
★★★☆☆
Ideal Batch Size
100s–1,000s pcs
Cost
$$$
Best for mid- to high-volume production, multi-shift operations
Note: Throughput rating – ★☆☆☆☆ = slow, ★★★★★ = fast; Wastage rating – ★☆☆☆☆ = high waste, ★★★★★ = minimal waste; Masking Requirement rating – ★☆☆☆ = high effort, ★★★★★ = low effort.

Presentations

Conformal Coatings

This presentation provides an introduction to conformal coatings and their role in protecting electronic assemblies from moisture, chemicals, dust, corrosion, and other environmental contaminants. It explores how conformal coatings can extend product life, common application methods, key limitations, and the various coating chemistries available, including acrylic, silicone, urethane, epoxy, and parylene systems. Attendees will gain a practical understanding of coating selection criteria and performance considerations for reliable electronics protection.


Presentations

Selection Guide for ABChimie Conformal Coatings

This presentation introduces the main types of conformal coatings provided by ABChimie and the process that should be used to select a product based on defined criteria.

Related Blogs

How to Select the Right Conformal Coating

How to Select the Right Conformal Coating

This blog guides you through selecting the right conformal coating by covering key chemistries, performance traits, and application methods. It includes a 30-day corrosive environment case study to illustrate real-world protection. A practical selector chart at the end helps you match coating characteristics to your specific requirements.

Chemical rework guide for acrylic conformal coatings

Chemical Rework Guide for Conformal Coatings

The article explains how acrylic conformal coatings can be selectively removed using solvents, making them one of the easiest coating types to rework. It describes the process of removing the coating from a targeted area, performing repairs or component replacement, and then recoating the assembly to restore environmental protection and reliability.

 
Moisture vapor permeability of conformal coatings on printed circuit boards (PCBs) and its impact on electronics protection and reliability

Why Moisture Vapor Permeability Matters in Conformal Coatings and PCB Reliability

Moisture vapor permeability (MVP) measures how easily water vapor can pass through a conformal coating, making it a critical factor in PCB protection. The article explains that even coatings that appear waterproof can allow moisture to diffuse through over time, potentially leading to corrosion, electrochemical migration, insulation resistance loss, and premature electronic failures.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers