STYCAST EFF 15

Harmonization Code : 3907300090 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms

LOCTITE STYCAST EFF 15

Main features

  • Excellent dielectric properties
  • Low stress
  • Low shrinkage

Product Description

LOCTITE STYCAST EFF 15 is an epoxy based free flowing syntactic foam powder is designed to be able to infiltrate around densely packed components and fill voids in electronic modules.

LOCTITE STYCAST EFF 15 exhibits low shrinkage during cure so that little stress is transmitted to the embedded components. This material self extinguishes after an external flame is removed.

Cure Schedule

  • 24 hours @ 100°C
  • 4 hours @ 120°C
  • 2 hours @ 150°C

Product Family

213289

1.8 lb - Pail | Yellow
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 35 days
CA Shipping in 12 weeks
EU Shipping in 55 days
Packaging
Unit of measure Pail
Net weight 0.68 kg
Gross weight 1.046 kg
Dimensions 17.3 x 17.3 x 19.7 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
0.24 g/cm3
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.12 W/m.K
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
7.9 kV/mm