MOLYKOTE 7

Harmonization Code : 2710199990 |

MOLYKOTE 7 RELEASE COMPOUND

Main features

  • 40 to 204 deg C Service Range
  • Release, Lubrication, Sealing, and Protection
  • 0.8% Evaporation at 200 deg C

Product Description

MOLYKOTE® 7 Release Compound is a white, translucent dimethyl silicone compound used for release, lubrication, sealing, and surface-protection applications involving plastics, rubber, metals, and adhesives. Its polydimethylsiloxane fluid and inert amorphous silica formulation maintains a serviceable consistency from -40 to 204°C (-40 to 400°F), while providing moisture resistance, electrical insulation, and low volatility. The non-curing compound can be applied by hand, brushing, wiping, or suitable automated equipment and is used in molding, rubber processing, cable installation, extrusion, and packaging equipment.

Key features

  • Broad service temperature range: Maintains a serviceable consistency from -40 to 204°C (-40 to 400°F).
  • Release and lubrication performance: Provides release, sealing, and rubber-lubrication properties for plastics, rubber, metals, and adhesive-contacting equipment.
  • Stable non-curing silicone compound: Resists moisture and oxidation, is practically nonvolatile, and shows little tendency to dry out during service.

Applications / Suitable for

  • Mold release for foundry shell and core molds
  • Break-in treatment for tire-press bladders
  • Rubber lubrication and preservation
  • Release applications involving adhesives and glues
  • Cable pulling of rubber-covered cable through conduit
  • Plastic extrusion and plastic-film packaging equipment

Technical Specifications

General Properties
Color
The color
white
Evaporation Rate
6.8
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.0
Thermal Properties
Operating Temperature
-40-204 °C
Electrical Properties
Arc Resistance
ASTM-D495 expresses arc resistance as the number of seconds that a material resists forming a surface-conducting path when exposed to a high-voltage, low-current arc occurring intermittently. Results obtained from a nominal 3 mm thickness are meant to represent the material’s reaction in any thickness.
126 s
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
17 kV/mm
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
2.8 x 10^15 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values are provided for product evaluation and are not intended as specification limits.

Property Value Unit Method / condition
Color White, translucent — CTM 0176
NLGI consistency 1 Grade CTM 0191
Worked penetration 270 mm/10 CTM 0191, 60 strokes
Worked penetration 322 mm/10 CTM 0191, 100,000 strokes
Specific gravity 1.0 — CTM 0022 at 25°C (77°F)
Shelf life At least 60 Months Stored at 25°C (77°F) from date of manufacture; refer to packaging for Use By date
Technical properties

After-processing / final-state properties

Typical in-use performance values are provided for product evaluation and are not intended as specification limits.

Property Value Unit Method / condition
Service temperature range -40 to 204 (-40 to 400) °C (°F) Serviceable consistency
Bleed 6.8 % CTM 0033A, 24 hr at 200°C (392°F)
Evaporation 0.8 % CTM 0033A, 24 hr at 200°C (392°F)
Dielectric constant 2.85 — CTM 0112 at 100 Hz
Dielectric constant 2.83 — CTM 0112 at 100 kHz
Dissipation factor <0.0001 — CTM 0112 at 100 Hz and 100 kHz
Dielectric strength >450 volts/mil CTM 0114, 50 mil gap
Volume resistivity 2.8 × 1015 ohm-cm At 23°C (73°F)
Arc resistance 126 Seconds CTM 0171

Leading Brands Trust in Our Products and Services