LOCTITE EA 9396

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite EA 9396

Main features

  • Low Mixed Viscosity
  • 120-Minute Pot Life
  • MMM-A-132 Type 1 Class 3 Qualification

Product Description

LOCTITE® EA 9396 AERO is a two-part, low-viscosity epoxy paste adhesive that cures at room temperature and develops high bond strength across test temperatures from -67°F to 350°F (-55°C to 177°C). The mixed adhesive has a viscosity of 35 Poise (3.5 Pa·s) at 77°F (25°C), a 120-minute pot life for a 100 g mass, and a 100:30 Part A-to-Part B mix ratio by weight. Normal performance can be developed through a 3-to-5-day cure at 77°F (25°C), while a 1-hour cure at 150°F (66°C) provides an accelerated option. The product is qualified to MMM-A-132, Revision A, Type 1, Class 3.

Key features

  • Low mixed viscosity: The mixed adhesive has a viscosity of 35 Poise (3.5 Pa·s) at 77°F (25°C).
  • Room-temperature processing: Provides a 120-minute pot life for a 100 g mass and develops handling strength after 24 hours at 77°F (25°C).
  • Temperature-dependent bond strength: ASTM D1002 lap-shear testing on phosphoric-acid-anodized 2024-T3 bare aluminum covers test temperatures from -67°F to 350°F (-55°C to 177°C).

Technical Specifications

Physical Properties
Viscosity (Part A)
70,000 mPa.s
Viscosity (Part B)
90 mPa.s
General Properties
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:30

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component, mixed-material, storage, and processing data for the two-part adhesive system.

Property Value Unit Method / condition
Color — Part A Blue — Uncured component
Color — Part B Purple — Uncured component
Color — Mixed Green to dark purple — Immediately after mixing
Viscosity — Part A 700 / 70 Poise / Pa·s 77°F/25°C; Brookfield HBT, spindle 4 at 10 rpm / 2.1 rad/s
Viscosity — Part B 0.9 / 0.09 Poise / Pa·s 77°F/25°C; Brookfield HBT, spindle 1 at 100 rpm / 10.5 rad/s
Viscosity — Mixed 35 / 3.5 Poise / Pa·s 77°F/25°C; Brookfield HBT, spindle 1 at 20 rpm / 2.1 rad/s
Density — Part A 1.17 g/mL Uncured component
Density — Part B 0.98 g/mL Uncured component
Density — Mixed 1.14 g/mL Mixed adhesive
Mix ratio — Part A:Part B 100:30 By weight Volume measurement is not recommended for structural applications unless ratio-control precautions are used
Pot life 120 minutes 100 g mass at 77°F/25°C; ASTM D2471, water bath
Handling strength 24 hours At 77°F/25°C; full bond strength has not yet developed
Normal cure 3–5 days At 77°F/25°C
Accelerated cure 1 hour At 150°F/66°C
Shelf life — Part A 1 year Stored below 40°F/4°C or below 77°F/25°C
Shelf life — Part B 1 year Stored below 40°F/4°C or below 77°F/25°C
Technical properties

After-processing / final-state properties

Typical cured adhesive and bonded-joint properties. Values remain specific to the listed cure, specimen, substrate, test method, and test temperature.

Property Value Unit Method / condition
Tensile lap shear strength 3,300 / 22.8 psi / MPa ASTM D1002; tested at -67°F/-55°C after 5 days at 77°F/25°C
Tensile lap shear strength 3,500 / 24.1 psi / MPa ASTM D1002; tested at 77°F/25°C after 5 days at 77°F/25°C
Tensile lap shear strength 3,200 / 22.0 psi / MPa ASTM D1002; tested at 180°F/82°C after 5 days at 77°F/25°C
Tensile lap shear strength 1,800 / 12.4 psi / MPa ASTM D1002; tested at 300°F/149°C after 5 days at 77°F/25°C
Tensile lap shear strength 1,250 / 8.6 psi / MPa ASTM D1002; tested at 350°F/177°C after 5 days at 77°F/25°C
Tensile lap shear strength 3,300 / 22.8 psi / MPa ASTM D1002; tested at -67°F/-55°C after 1 hour at 150°F/66°C
Tensile lap shear strength 4,000 / 27.6 psi / MPa ASTM D1002; tested at 77°F/25°C after 1 hour at 150°F/66°C
Tensile lap shear strength 3,300 / 22.8 psi / MPa ASTM D1002; tested at 180°F/82°C after 1 hour at 150°F/66°C
Tensile lap shear strength 1,800 / 12.4 psi / MPa ASTM D1002; tested at 300°F/149°C after 1 hour at 150°F/66°C
Tensile lap shear strength 1,200 / 8.3 psi / MPa ASTM D1002; tested at 350°F/177°C after 1 hour at 150°F/66°C
Tensile lap shear strength 3,500 / 24.1 psi / MPa ASTM D1002; tested at -67°F/-55°C after 30 minutes at 180°F/82°C
Tensile lap shear strength 4,000 / 27.6 psi / MPa ASTM D1002; tested at 77°F/25°C after 30 minutes at 180°F/82°C
Tensile lap shear strength 3,300 / 22.8 psi / MPa ASTM D1002; tested at 180°F/82°C after 30 minutes at 180°F/82°C
Tensile lap shear strength 1,900 / 13.1 psi / MPa ASTM D1002; tested at 300°F/149°C after 30 minutes at 180°F/82°C
Tensile lap shear strength 1,200 / 8.3 psi / MPa ASTM D1002; tested at 350°F/177°C after 30 minutes at 180°F/82°C
Bell peel strength 25 / 111 lb/in / N/25 mm ASTM D3167; tested at 77°F/25°C after 5 days at 77°F/25°C
Bell peel strength 20 / 89 lb/in / N/25 mm ASTM D3167; tested at 180°F/82°C after 5 days at 77°F/25°C
Service temperature Approximately 350 / 177 °F / °C Defined as the temperature at which the adhesive retains 1,000 psi/6.9 MPa by ASTM D1002
Tensile strength 8,000 / 35.2 psi / MPa ASTM D638; 0.125 in/3.18 mm casting; tested at 77°F/25°C; cure 5 days at 77°F/25°C plus 1 hour at 200°F/93°C
Tensile modulus 400,000 / 2,750 psi / MPa ASTM D638; 0.125 in/3.18 mm casting; tested at 77°F/25°C; cure 5 days at 77°F/25°C plus 1 hour at 200°F/93°C
Elongation at break 3.4 % ASTM D638; tested at 77°F/25°C; cure 5 days at 77°F/25°C plus 1 hour at 200°F/93°C
Dielectric constant 4.17 — ASTM D150 at 0.1 kHz
Dielectric constant 4.12 — ASTM D150 at 1.0 kHz
Dielectric constant 3.97 — ASTM D150 at 10.0 kHz
Dissipation factor 0.006 — ASTM D150 at 0.1 kHz
Dissipation factor 0.017 — ASTM D150 at 1.0 kHz
Dissipation factor 0.031 — ASTM D150 at 10.0 kHz
Volume resistivity 2.14 × 1015 Ω·cm Electrical property testing per ASTM D149/D150
Surface resistivity 3.17 × 1014 Ω Electrical property testing per ASTM D149/D150
Thermal conductivity 5.01 × 10-4 cal/(s·cm·°C) Cured bulk resin property
Coefficient of thermal expansion, α 70.7 µm/m·°C Measured at 40°C
Coefficient of thermal expansion, α 108.0 µm/m·°C Measured at 100°C
Hardness 80 Shore D Measured at 77°F/25°C

Lap-shear and peel specimens used 2024-T3 bare aluminum adherends phosphoric-acid anodized in accordance with ASTM D3933.