LOCTITE E-60HP

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE E-60HP

Main features

  • Extended 60-Minute Working Life
  • Toughened Structural Epoxy Bonding
  • Electrical-Insulating Cured Bondline

Product Description

LOCTITE EA E-60HP is a two-part, toughened structural epoxy adhesive with medium viscosity, extended working life and room-temperature cure. The resin and hardener mix 2:1 by volume and provide a 60-minute working life at 23 deg C, supporting assembly adjustment before cure. After a five-day cure at 23 deg C, the adhesive develops high lap-shear strength on prepared metal substrates together with electrical-insulating and mechanical properties. It is intended for high-performance structural bonding across supported engineering substrates where a longer processing window is more important than rapid fixture.

Key features

  • Extended work life: Provides a 60-minute working life at 23 deg C for assembly adjustment before cure.
  • Toughened room-temperature cure: Two-part medium-viscosity epoxy cures at room temperature to a tough off-white bondline.
  • Steel and Aluminum Bond Strength: Typical lap shear strength is 30 N/mm^2 under ISO 4587 on grit-blasted mild steel and acid-etched, abraded aluminum after a five-day cure at 23 deg C.

Applications

Structural bonding applications requiring high performance and extended work life across supported engineering substrates.

Technical Specifications

General Properties
Appearance
Off-white
Pot Life
60 minutes
Specific Gravity
1
Physical Properties
Tack-Free Time
120 minutes
Thermal Properties
Glass Transition Temperature (Tg)
70 °C
Mechanical Properties
Elongation
9 %

Additional Information

Technical properties

As-supplied properties

PropertyValueUnitMethod / condition
Mix ratio by volume2:1Resin:hardener
Mix ratio by weight100:50Resin:hardener
Resin viscosity67,500mPa sBrookfield RVT; spindle 7; 20 rpm; 25 deg C
Hardener viscosity7,000mPa sBrookfield RVT; spindle 6; 50 rpm; 25 deg C
Working life60min23 deg C
Tack-free time120min23 deg C
Technical properties

Final-state properties

PropertyValueUnitMethod / condition
Glass transition temperature70deg CTMA; ISO 11359-2; cured 5 days at 23 deg C
Hardness80Shore DISO 868; cured 5 days at 23 deg C
Elongation9%ISO 527-3; cured 5 days at 23 deg C
Tensile strength35N/mm^2ISO 527-2; cured 5 days at 23 deg C
Dielectric breakdown strength13kV/mmIEC 60243-1; cured 5 days at 23 deg C
Lap shear strength30N/mm^2Grit-blasted mild steel; cured 5 days at 23 deg C
Lap shear strength30N/mm^2Acid-etched and abraded aluminum; cured 5 days at 23 deg C