Sample Kit | Linqstat VCF, MVCF & XVCF Conductive and Antistatic Films

Harmonization Code : 3920.10.28.99 | Polymers of Ethylene Plates, Sheets, Film, Foil, Tape, or Strips (Non-cellular), having a thickness not exceeding 0.125mm, having a specific gravity of 0.94 or more

Sample Kit | Linqstat VCF, MVCF & XVCF Conductive and Antistatic Films Linqstat VCF, MVCF & XVCF Conductive and Antistatic Film Sample Kit Linqstat VCF - Antistatic Linqstat MVCF - Carb Linqstat XVCF - TENS Electrodes

Main features

  • LINQSTAT Sample Kit
  • Complete package with Conductive and Antistatic
  • Carbon loaded PE film with low surface resistivity

Product Description

We offer a range of carbon loaded polyethylene (PE) based LINQSTAT-branded electrically conductive and antistatic plastic film. Our electrically conductive plastics start with a surface resistivity of less than 200,000 ohm-per-square and can go as low as 200 ohms-per-square.

LINQSTAT™ VCF, MVCF and XVCF Series electrically conductive plastic sheeting is a black, carbon-filled, volume-conductive polyethylene film designed to provide both physical and static protection in numerous semiconductor, electronics, and Smartcard applications. The different grade of materials allows users to cover a wide range of possible applications.

A common application of the conductive polyethylene films is as a pressure sensor. The LINQSTAT MVCF films can be used as a weak pressure sensor making it useful for applications that have large surface areas and expect large pressure applications. The LINQSTAT XVCF films are used for more sensitive pressure sensor applications. LINQSTAT VCF with lower conductivity levels are perfect for antistatic packaging plastic, for example as an antistatic interleaver for smartcard (micromodule) applications. It’s antistatic properties make the Linqstat films also well suited for EMI and RF shielding applications.

The Sample package includes 1 A4 size sheet of:

Sample kit contents are subject to change based on stock availability at the time of order.

Product Family

230966

Linqstat XVCF & MVCF Sample Kit - Conductive Package
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Kit
Net weight 0.056 kg
Gross weight 0.38 kg
Dimensions 30 x 22 x 1 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Carbon-Loaded PE
Color
The color
Black
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.10-1.18
Other Properties
RoHS Compliant
RoHS is a product level compliance based on a European Union Directive which restricts the Use of certain Hazardous Substances in Electrical and Electronic Equipment (RoHS). Products compliant with this directive do not exceed the allowable amounts of the following restricted materials: lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls (PBB) and polybrominated diphenyl ethers (PBDE), with some limited exemptions
Yes