ENTHONE CAT 20/A

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

ENTHONE 20/A

Main features

  • Two-Hour Mixed-Ink Pot Life
  • Ambient or Heat Cure
  • Permanent Marking Application Flexibility

Product Description

ENTHONE Catalyst 20/A is an ambient- or heat-cure catalyst component for ENTHONE M-Series and 50-Series two-component epoxy marking inks. With the selected ink, the mixture has an average 2-hour pot life after a 30-minute induction period. A room-temperature air cure reaches tack-free condition in approximately 1 to 2 hours and develops over 5 to 7 days, while heat cure is also available. The catalyst supports permanent marking processes for semiconductor components, printed circuit boards, connectors, dials, nameplates, panels, chassis, glass, and compatible plastics.

Key features

  • Two-Hour Mixed Pot Life: The ink and Catalyst 20/A mixture has an average 2-hour pot life after induction.
  • Ambient or Heat Cure: The selected ink system may cure at room temperature or through a heat-assisted schedule.
  • Multi-Method Marking: Compatible inks may be stamped, screen printed, sprayed, brushed, or roller printed.

Applications / Suitable for

  • Permanent marking of semiconductor components
  • Printed circuit boards, connectors, and dials
  • Nameplates, panels, chassis, glass, and compatible plastics

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Basic air cure catalyst

Additional Information

Technical properties

As-supplied / before-processing properties

Typical processing data for Catalyst 20/A used with M-Series or 50-Series epoxy marking inks.

Property Value Unit Method / condition
Induction period 30 minutes Ink/catalyst mixture before application
Average pot life 2 hours Catalyst 20/A with M-Series or 50-Series ink; begins after induction
Tack-free time 1 to 2 hours Room-temperature air cure; depends on ink film thickness
Room-temperature cure 5 to 7 days Catalyst 20/A with ENTHONE epoxy marking ink
Cure mode Room temperature or heat - Catalyst 20/A may be fully or partially heat cured
Catalyst shelf life 2 years From date of manufacture
Moisture handling Keep tightly closed - Catalysts are hygroscopic

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers