ECCOSHIELD-VY
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Non-Hardening Conductive RF-Seam Compound
- 0.001 ohm-cm Volume Resistivity
- 40 to 288 deg C Service Range
Product Description
ECCOSHIELD® VY Conductive Caulking Compound is a single-component, metallic-particle-filled, electrically conductive sealer for radio-frequency-shielded structures. The non-hardening compound is applied with conventional caulking equipment to fill and seal seams, joints, cabinet interfaces, conduit connections, and threaded areas requiring electrical continuity. It remains pliable after application and is documented for structures exposed to vibration, temperature change, or joint displacement. Typical data include 0.001 ohm·cm volume resistivity, service from -40°C to 288°C, and insertion loss greater than 100 dB at a caulked joint.
Key features
- Non-hardening conductive seal: The single-component caulking compound remains pliable after application.
- Low volume resistivity: Typical volume resistivity is 0.001 ohm·cm.
- RF shielding performance: Documented insertion loss is greater than 100 dB at a caulked joint.
Applications / Suitable for
- Radio-frequency-shielded cabinets and structures
- Seams, joints, conduit connections, and threads
- Removable covers requiring conductive sealing
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Electrical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied values unless otherwise stated. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product form | Single-component non-hardening caulking compound | N/A | As supplied |
| Density | 4.9 | g/cm³ | As supplied |
| Bead yield | 33.5 | m/kg | 3 mm diameter bead |
| Minimum application temperature | 20 | °C | Recommended application condition |
After-processing / final-state properties
Typical final-state values under the stated conditions. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Volume resistivity | 0.001 | ohm·cm | Typical applied material |
| Service temperature range | -40 to 288 | °C | Documented operating range |
| Insertion loss | >100 | dB | Measured at a caulked joint |