DOWSIL 3145
Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics
Main features
- Military-grade
- High strength
- Non-flowing paste
Product Description
DOWSIL™ 3145 RTV MIL-A-46146 Adhesive Sealant is a high-strength, one-part silicone solution available in clear and gray, specifically engineered for the rigorous demands of military and aerospace electronics. This non-flowing (non-sag) paste cures at room temperature upon exposure to atmospheric moisture, eliminating the need for curing ovens. Designed to provide long-term bonding and protection against mechanical shock, vibration, and thermal cycling, it maintains exceptional stability across a broad temperature range of -50°C to +200°C.
Product Key Features
- Military Grade: fully meets the requirements of MIL-A-46146 Group II/III, Type I specifications.
- High Strength: delivers exceptional tensile strength (up to 1,035 psi) and high elongation (up to 670%) for durable structural bonds.
- Non-Flowing Paste: non-sag consistency allows for precise application on vertical or overhead surfaces without slumping.
- Thermal Stability: remains flexible and stable from -50°C up to +200°C, with the gray version offering even higher thermal limits.
- Excellent Dielectric Properties: provides reliable electrical insulation for sensitive electronic sub-assemblies.
- Easy Processing: one-part moisture cure system requires no mixing and features a tack-free time of approximately 60–90 minutes.
- Primerless Adhesion: formulated to bond well to many reactive metals, glass, ceramics, and silicone rubber.
Key Applications
- Sealing openings in modules, housings, and aircraft panels.
- Adding mechanical stability to individual components on Printed Wiring Boards (PWBs).
- Sealing in and around wired leads and electrical connectors to prevent environmental contamination.
- Aviation MRO and AOG repairs requiring rapid, high-strength sealing.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Electrical Properties
Thermal Properties
Additional Information
DOWSIL 3145 RTV MIL-A-46146 Adhesive Sealant - Clear
A clear, one-part PDMS adhesive sealant with a non-flowing consistency and room-temperature moisture cure. It is documented for module and housing sealing, PWB component assembly, and sealing around wired and electrical leads. Typical cured data combine high elongation with tensile, tear, and dielectric performance, and the product is identified as MIL-A-46146 Group II, TY I.
Typical application and handling properties
Typical values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| One or two-part | One | - | As supplied |
| Color | Clear | - | As supplied |
| Extrusion rate | 78.6 | g/min | Typical value |
| Viscosity | 862 | Pa-sec | Low shear, 1/s |
| Viscosity | 168 | Pa-sec | High shear, 10/s |
| Flow rate - slump | 0.092 | in | Typical value |
| Tack-free time | 63.8 | minutes | 25 deg C |
| NVC (non-volatile content) | 96.9 | % | Typical value |
Room-temperature moisture cure
DOWSIL 3145 RTV cures from the exposed surface inward using moisture in the air. Surface preparation, open exposure to atmospheric moisture, and section geometry are important processing considerations.
Preparation and application sequence
Protect the material from moisture during storage
Store at or below the storage temperature listed on the product label in the original package with the cover tightly attached. Minimize moisture exposure and headspace; partially filled containers should be purged with dry air or another dry gas such as nitrogen. Use the product by the Use Before date shown on the label.
Technical guidance for product evaluation
Mechanical and electrical properties
Typical cured values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Specific gravity | 1.10 | - | Cured |
| Tensile strength | 864 | psi | Typical cured value |
| Elongation | 626 | % | Typical cured value |
| Tensile modulus | 138 | psi | Typical cured value |
| Tear strength | 223 | ppi | Die B |
| Durometer | 45.6 | Shore A | Typical cured value |
| Unprimed adhesion - lap shear to aluminum | 336 | psi | Equivalent source values: 2.32 MPa and 232 N/cm^2 |
| Dielectric strength | 485 | volts/mil | Typical cured value |
| Volume resistivity | 4.4 E+14 | ohm*cm | Typical cured value |
| Dielectric constant | 2.83 | - | 100 Hz |
| Dielectric constant | 2.83 | - | 100 kHz |
| Dissipation factor | 0.0005 | - | 100 Hz |
| Dissipation factor | < 0.0002 | - | 100 kHz |
Documented electronics sealing and assembly uses
The supplied TDS identifies three application areas for DOWSIL 3145 RTV. Final substrate, geometry, cure access, and service conditions should be evaluated for the specific assembly.
Evaluate DOWSIL 3145 RTV for your assembly
Contact Krayden to discuss substrate compatibility, moisture-cure access, dispense approach, service-temperature conditions, or MIL-A-46146 documentation for your specific assembly. The technical team can also help review whether the documented mechanical and dielectric properties align with your application and qualification requirements.