CS-783 | Methacrylated Epoxy Functional Hybrid Cyclosiloxane

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

CS-783 | Methacrylated Epoxy Functional Hybrid Cyclosiloxane

Main features

  • Low viscosity
  • Dual cure mechanism
  • Multifunctional

Product Description

DMI CS-783 is a methacrylated, epoxy-functional hybrid cyclosiloxane monomer engineered to enhance adhesion and compatibility in advanced resin systems. Its unique structure allows participation in both free-radical polymerization and epoxy curing mechanisms, offering broad versatility for formulating high-performance adhesives, coatings, and composite materials.

Used primarily as an adhesion promoter for mold compounds, metal surfaces, and polyimides, DMI CS-783 improves interfacial bonding without sacrificing processing ease. Additionally, it serves as a multifunctional diluent, reducing viscosity and enhancing flow properties across a wide range of resin systems. Soluble in most common resins, DMI CS-783 simplifies formulation without compromising performance.

Applications

  • Adhesion promoter for mold compounds, metals, and polyimide surfaces
  • Reactive diluent for epoxy, hybrid, and UV-curable systems
  • Formulations requiring dual-cure compatibility (free-radical and epoxy cures)
  • B-staged and hybrid adhesives, coatings, and composites
Product Family

233971

1kg jar
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Jar
Net weight 1 kg
Gross weight 1.3 kg
Dimensions 10 x 10 x 20 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Yellow liquid
Molecular weight
783 g/mol
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
250 mPa.s

Additional Information

Recommended Formulation Use

  • CS-783 is recommended for use as an adhesion promoter to mold compounds and metal substrates. Typical addition  levels are 1-5% of the total resin. CS-783 can also be used for standard epoxy curatives, catalysts, B-staged and/or hybrid adhesives. 

Property

Value

Unit

Physical and Chemical Properties

Epoxy functionality

2-4

-

Methacrylate functionality

1-2

-

Average epoxy equivalent weight

261

-

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers