ABLESTIK 2113

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE ABLESTIK 2113

Main features

  • Low-Viscosity Optical Bonding
  • Fine-Detail Flow and Wetting
  • Electrically Insulating Cured Adhesive

Product Description

LOCTITE ABLESTIK 2113 BIPAX is a two-component, transparent, non-conductive epoxy adhesive supplied at a 100:11 resin-to-hardener mix ratio in a BIPAX mixing-dispenser package. Formulated for applications requiring low initial viscosity and near-transparent color, it offers excellent flow and wetting properties for fine detail work and difficult-to-reach bond lines. This solvent-free system cures at room temperature over 24 hours or faster at 65°C, and supports continuous service from -60°C to 130°C. It is recommended for fiber optic assembly, structural laminating, and high-performance aerospace and electronic applications, bonding glass, ceramics, metals, and plastics with good chemical resistance and electrical insulation.

Key features

  • Low viscosity, transparent: 300 mPa·s mixed viscosity with near-transparent cured appearance for optical clarity needs.
  • Excellent flow and wetting: Supports fine detail bonding and fiber optic assembly applications.
  • Electrically insulating: Dielectric strength of 410 volts/mil for demanding electronic applications.

Applications / Suitable for: Fiber optic assembly, structural laminating, and high-performance aerospace and electronic applications.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Transparent
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.16
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
1
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
300 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
77 °C
Operating Temperature
-60 to 130 °C
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
60000000000000 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured, mixed material prior to cure.

Property Value Unit Method / condition
Mix ratio (Resin : Hardener) 100 : 11 by weight —
Viscosity, mixed 300 mPa·s (cP) @ 25°C, mixed
Specific gravity, mixed 1.16 — Mixed material
Pot life 30 minutes Mixed material
Technical properties

After-processing / final-state properties

Typical properties of the fully cured material after the recommended cure schedule.

Property Value Unit Method / condition
Hardness 88 Shore D Cured material
Glass transition temperature (Tg) 77.0 °C Cured material
Dielectric strength 410 volts/mil Cured material
Volume resistivity 6.00×10¹³ ohm·cm @ 25°C
Lap shear strength, Al to Al 15 (2,200) N/mm² (psi) Sample cured 2 hr @ 65°C